Thermal Ceramics Blanket FireMaster

 

Material Notes:
FireMaster Blanket is a high-temperature fiber blanket which is classified by Underwriters Laboratories under “Batts and Blankets (BKNV)” in the UL Building Materials Directory, No. R8418. FireMaster Blanket is manufactured to ensure continued compliance with certification standards. The blanket is used as a fireproof covering or wrap. Foil facing or encapsulation is available in aluminum or stainless steel to reduce the risk of physical damage, minimize dusting, and protect against weathering.

Features:

  • UL-classified, noncombustible material
  • Lightweight/flexible
  • Optional foil facing or encapsulation
  • Low thermal conductivity
  • Resists chemical attack
  • Unaffected by oil or water
  • Completely inorganic
  • Excellent acoustical properties
  • Applications:

  • OEM manufactured systems such as fire doors and panels
  • Up to 3 hour cable tray, conduit, and through penetration firestops
  • Structural steel
  • Plastic pipes
  • Above ground storage tanks
  • Railcar tanks
  • Motor Operated Valves
  • Information provided by Thermal Ceramics

    Available Properties
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Flammability Test
    • Water Leachable Elements on Surface of Fiber, PPM
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。