Thermal Ceramics Marine Blanket FireMaster

 

Material Notes:
FireMaster Marine Blanket is a lightweight, non-combustible mat that is produced from a calcium- magnesium-silicate raw material. There are no organic binders present in this mechanically needled mat producing no smoke or flame during a fire condition and maintains good surface integrity and strength. This fiber technology is soluble within the human body and provides excellent thermal and acoustic properties.

Features:

  • UL classified R8418, Non-combustibility per ISO 1182
  • US Coast Guard, DNV, and ABS approved for structural fire protection of IMO high speed craft and SOLAS commercial vessels
  • DNV and Lloyds approved for off-shore platform hydrocarbon bulkhead and deck applications
  • Up to 50% weight and installed savings over mineral wool
  • Aluminum and steel bulkhead and deck systems: A30, A60, and H60 Bulkhead and Deck structural insulation
  • Mechanical abuse and oil spray protection facings available
  • Inert and resistant to mold growth and attack of vermin
  • Applications:

  • A30 - Aluminum Bulkhead/Decks
  • A60 - Aluminum Bulkhead/Decks
  • A30-Steel Bulkhead/Decks
  • A60-Steel Bulkhead/Decks
  • H60-Steel Bulkhead/Decks
  • Marine fire doors
  • Marine exhaust pipes
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Flammability Test
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。