Thermal Ceramics 1401 Kaowool Millboard

 

Subcategory: Kaolin

Material Notes:
Kaowool 1401 Millboard is a strong, thin, dense board product with excellent compression resistance and insulating characteristics. It is produced from Kaowool ceramic fibers, clay, inert fillers, and a small amount of both organic and inorganic binders for increased handling strength. It maintains its integrity throughout a wide temperature range and is easily fabricated and die cut. Kaowool Grade 1401 Millboard is an excellent product for backup insulation and many types of gasketing applications.

Features:

  • Asbestos replacement millboard
  • Thin durable insulation and gasketing
  • Easy to die cut
  • Good compression resistance
  • Excellent dimensional stability
  • Excellent backup insulation
  • Applications:

  • High-temperature gaskets
  • Heat and flame shields
  • Parting media
  • Thermal barrier
  • Refractory backup insulation
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Modulus of Rupture
    • Compressive Strength
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Moisture Content
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。