Thermal Ceramics 2600E RPC Shapes

 

Material Notes:
RPC 2600 is an insulating material produced by blending alumina-silicate fibers and polycrystalline fibers with high purity silica binders. The alumins fibers form a matrix within the material, and give it high temperature capability. The high temperature capability is further enhanced by employing ammonia stabilized colloidal silica rather than sodium stabilized product. At elevated temperatures, residual sodium acts as a flux and reduces the refractories maximum use temperature.

Features:

  • No organic binders
  • Complex shape capability
  • Low thermal conductivity and minimal heat storage
  • High resistance to thermal shock and spalling
  • Low shrinkage
  • Light weight
  • Applications:

  • Bullnose tiles
  • Burner blocks
  • Combustion chamber construction
  • Diffusion furnaces
  • Flue and exhaust stack liners
  • Furnace components
  • General molten metal contact
  • Peep door frames and plugs
  • Heat shields
  • High temperature gaskets and seals
  • Hot tops for super alloy casting
  • Molten aluminum contact
  • Semiconductor processing equipment
  • Shapes for laboratory furnaces
  • Shapes in ammonia reformers
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Modulus of Rupture
    • Compressive Strength
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。