Thermal Ceramics RPC™ 2300-W Wet Felt

 

Material Notes:
Wet Felt is a high-alumina, ceramic fiber material made by a vacuum forming process that produces a unique insulating process capable of withstanding 2300°F (1260°C). Bonded with our standard bond, it has virtually unlimited uses. It is shipped wet in sheets, rolled or flat, and sealed in protective plastic bags. Standard sizes are 48 x 36 x 1/8 to 1" (1200 x 900 x 3.125 to 25mm) thick.

Features:

  • Non-self sticking and can be joined by air-set mortar
  • Drying time is 24 to 48 hours
  • Maintains wet shape and characteristics of prefired material after drying
  • Random fiber orientation and a tightly knit structure
  • Collodial silica is disbursed uniformly throughout the entire piece and does not drain out
  • Does not require costly dryers, tooling or machining to conform to size requirements
  • Applications:

  • Wrapping exhaust manifolds in marine engines
  • Wrapping fuel injector nozzles in solid fuel fired kilns
  • Lining combustion duct work in incinerators and boilers
  • Lining hot tuyers in upcomers of blast furnaces
  • Hand packed to protect the anchor of an element hanger module
  • Information provided by Thermal Ceramics

    Available Properties
    • Hardness, Shore A
    • Modulus of Rupture
    • Compressive Strength
    • Specific Heat Capacity
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。