Thermal Ceramics Therm-O-Hot Patch™

 

Material Notes:
Therm-O-Hot Patch and Therm-O-Hot Patch HS are ideal insulating materials for fast, easy, refractory repairs. Therm-O-Hot Patch is composed of exfoliated vermiculite with binders and is a heat-set product. Therm-O-Hot Patch HS is similar to the regular grade but contains an additional binder to make it a strong, air-set product. They have a service range to 1900°F (1040°C), are premixed, and shipped in a five gallon pail. Both can be used for joints, cracks in walls, arches, and furnace roofs to stop heat leaks. Therm-O-Hot Patch and Therm-O-Hot Patch HS both make an excellent seal for “hot” walls, bulkheads and arches, minimizing cold air infiltration, and conserving heat loss.

Simply open the pail, and depending upon the method of application required, pump, caulk, spray, or trowel in place. Therm-O-Hot Patch and Therm-O-Hot Patch HS both adhere well to all surfaces and dry quickly with minimal shrinkage.

Features:

  • Service range to 1900°F (1038°C)
  • Excellent for fast, easy, hot surface repairs
  • Adheres well to all surfaces
  • Dries quickly
  • Indefinite shelf life on standard Therm-O-Hot Patch
  • Applications:

  • On the spot repair jobs to side walls, end walls, ports or furnace roofs
  • A sealer for “hot” walls, bulkheads, and arches
  • Reduce cold air infiltration
  • Reduce heat loss
  • Good for expansion joint areas
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Compressive Strength
    • Thermal Conductivity
    • Maximum Service Temperature, Air
    • Shrinkage
    • Cr2O3 content
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。