Thermal Ceramics 607 PM Superwool Board

 

Material Notes:
Superwool 607 PM boards are processed from a slurry consisting of Superwool bulk and organic binders. This board product is noted for its excellent surface finish, thickness uniformity and high insulating value at elevated temperatures.

Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalies (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying.

The non-wetting characteristics of the Superwool 607 PM Board composition make is an excellent alternative for molten aluminium contact.

Features:

  • Continuous temperature rating of 1832°F
  • Low thermal conductivity and heat storage
  • Very close thickness tolerance
  • Excellent surface finish and uniformity
  • Easily fabricated and die-cut
  • Applications:

  • Appliance and heat processing equipment insulation
  • Combustion chamber construction for domestic appliance construction
  • Heat shields
  • High temperature gaskets and seals
  • Back-up insulation to dense refractories
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Modulus of Rupture
    • Compressive Strength
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。