Zircar Zirconia ZYK-15 Zirconia Cloth

 

Subcategory: Oxide, Zirconium; Oxide

Key Words: ZrO2, zirconium oxide

Material Notes:
Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexible form and provides the lowest thermal conductivity of any commercially available refractory fiber material. ZYK-15 cloth is ideal for temperatures up to 2200°C. The melting temperature is 2590°C. It is suitable for applications such as high energy battery separators, thermal insulation in crystal growing furnaces, and for the filtration of hot gases.

ZYK-15 is a true textile constructed of essentially continuous individual filaments fabricated in a tricot knit form. It requires neither binders nor supporting wires in its construction and will comply somewhat to both tensile and compressive forces due to the mechanical interlocking of their fibers. Elongation of 4 to 8% before breaking allows ZYK-15 to conform to irregular surfaces. ZYK-15 can be compressed up to two-thirds of its normal thickness and still recover a major fraction of its original dimension with little fiber damage.

The fine capillary and pore structure of ZYK-15, in combination with the hydrophilic nature of zirconia and the serrated surface of the individual fibers in the knit threads, impart excellent wetting solution retention and wicking characteristics to this material.

Features:

  • Low Thermal Conductivity
  • High Purity
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Can be Cemented with Zircar Zirconia Cement Type ZR-CEM
  • Can be Rigidized with Zircar Zirconia Rigidizer Type ZR-RIG
  • Easily Cut to Size
  • Available ‘off the shelf’

Information provided by Zircar Zirconia.

Available Properties
  • Bulk Density
  • Porosity
  • Thickness
  • Vapor Pressure
  • Specific Heat Capacity
  • Melting Point
  • Maximum Service Temperature, Air
  • Shrinkage
  • Tensile Strength per Unit Width
  • Trace Impurities
  • Weight Per Area
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。