Zircar Zirconia ZOF-100 Pure Zirconia Felt

 

Subcategory: Oxide, Zirconium; Oxide

Key Words: ZrO2, zirconium oxide

Material Notes:
Zircar’s unique process for manufacturing yttria-stabilized zirconia cloths and felts is also used in the production of pure zirconia refractory fibers and textiles without stabilizers. For those processes which are intolerant of yttria, these unstabilized pure zirconia fiber products provide much of the same high performance insulating benefits. Pure zirconia fibers exist in the monoclinic crystal phase and appear white in color. Our high purity zirconia fiber and textiles are offered in six different standard product forms; bulk fiber Type ZOBF, two felts Types ZOF-50 and ZOF-100 and three types of knit cloth Types ZOK-15, ZOW-15 and ZOW-30.

Features:

  • High Purity Zirconia
  • High Temperature Stability
  • Low Thermal Conductivity
  • Excellent Thermal Shock Resistance
  • No Outgassing
  • Six Different Product Formats Offered
  • Available ‘Off the Shelf’

Application Information:

  • Pure zirconia cloth is used as high temperature insulation for advanced energy systems.

Information provided by Zircar Zirconia.

Available Properties
  • Loss On Ignition
  • Outgassing - Total Mass Loss
  • Melting Point
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。