ZIRCAR Ceramics MICROSIL Microporous Insulation

 

Subcategory: Oxide, Silicon; Oxide

Material Notes:
MICROSIL Microporous Insulation is an incredible insulation material. Having thermal conductivity an order of magnitude lower than ceramic fiber materials Microsil Microporous Insulation can be an integral part of thousands of thermal management applications with temperatures as high as 950C (1742F). MICROSIL is a combination of ultra-fine silica powders, specially processed refractory oxides and glass reinforcing fibers. Compacted under tons of force to form a light weight yet rigid structure MICROSIL offers maximum insulation in a minimum amount of space, saving weight and most importantly energy. Unique to MICROSIL's microporous structure is its low density which minimizes conductive heat transfer and its billions of nano-pockets which block convection and reflect heat energy – like mirrors – back to its source. MICROSIL is nearly immune to thermal shock. It is completely non-combustible in accordance with standard DIN 4102 Class A1 and can be stored indefinitely in dry conditions. MICROSIL's microporous structure is adversely effected by water, oil, alcohol and other liquids.

Information provided by Zircar.

Available Properties
  • Density
  • Compressive Strength
  • Compression Set
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Maximum Service Temperature, Air
  • Shrinkage
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。