American Elements Lanthanum Oxide Nanopowder

 

Subcategory: Oxide, Other; Oxide

Key Words: Formula: La2O3; CAS Number: 1312-81-8

Material Notes:
General Description

Lanthanum Oxide (LaO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Lanthanum Oxide Particles are typically 10-30 nanometers (nm) with specific surface area (SSA) in the 130-150 m 2 /g range. Nano Lanthanum Oxide Particles are also available in passivated and in Ultra high purity and high purity and carbon coated and dispersed forms. Applications for Lanthanum Oxide nanocrystals include in preparation of various perovskite nanostructures (such as lanthanum manganite and lanthanum chromite) for the cathode layer of solid oxide fuel cells (SOFC), as a Magnetic Nanoparticle (also as iron oxide -lanthanum oxide nanoparticles) for magnetic data storage and magnetic resonance imaging (MRI), in biosensors, for phosphate removal in bio medical and water treatment (including swimming pools and spas) applications, in laser crystals and optics, and in nanowire, nanofiber and in certain alloy and catalyst applications. Further research is being done for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience uses.

Available Properties
  • Density
  • Particle Size
  • Specific Surface Area
  • Molecular Weight
  • Melting Point
  • Boiling Point
  • Appearance
  • Solubility
  • Stability
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。