American Elements Rhenium Nanoparticles

 

Subcategory: Pure Element; Nonferrous Metal

Key Words: Formula: Re; CAS Number: 7440-15-5

Material Notes:
General Description

Rhenium (Re) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Rhenium Particles are typically 20 - 100 nanometers (nm) with specific surface area (SSA) in the 1 – 3 m 2 /g range. Nano Rhenium Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Rhenium nanocrystals include for immunotherapy of solid tumors, in a nucleation layer of palladium and rhenium nanoparticles in-between a nanostructure copper pad surface to create an electrical connection that has superior diffusion barrier and adhesion properties numerous uses in catalysts, in magnetically targeted therapy and as a Magnetic Nanopowder, in polymer membranes to create Active Polymer Membranes and in other coatings, plastics, nanofiber and textiles and in nanowire and other catalysis applications.

Available Properties
  • Particle Size
  • Specific Surface Area
  • Molecular Weight
  • Appearance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。