American Elements Zirconium Oxide Nanopowder

 

Subcategory: Oxide, Zirconium; Oxide

Key Words: Formula: ZrO2; CAS Number: 1314-23-4

Material Notes:
General Description

Zirconium Oxide or Zirconia Nanopowder or Nanoparticles (ZrO2), nanodots or nanocrystals are white high surface area particles available in monoclinic or as stabilized or doped with yttria (yttrium oxide), calcia (calcium oxide), or magnesia (magnesium oxide), or phosphorized zirconia. Nanoscale Zirconium Oxide Nanoparticles are typically 5 - 100 nanometers (nm) with specific surface area (SSA) in the 25 – 50 m 2 /g range. Nano Zirconium Oxide Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Zirconium oxide or zirconia nanocrystals include as a support for active catalytic metals, such as ceria and platinum (ceria-zirconia nanoparticles), in micro-ceramics, when doped with yttria in solid oxide fuel cell (SOFC) electrolyte microlayers, to absorb radionucletides, and in coatings, plastics, nanowire, nanofiber and textiles and in certain bioscience applications.

Available Properties
  • Density
  • Particle Size
  • Specific Surface Area
  • Molecular Weight
  • Melting Point
  • Appearance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。