Poco Graphite Fabmate® Pore-Free Specialty Graphite

 

Subcategory: Graphite; Carbon

Material Notes:
Shore scleroscope C-2 hardness is 77. FABMATE is the trade name for a high-strength, finished product that has been purified, machined and subjected to Poco Graphite's proprietary carbon modification treatment.

FABMATE products are designed for use in clean rooms. They are ideal for semiconductor applications requiring exceptional cleanliness and a pore-free surface.

The graphite substrate is fine-grained, high strength graphite that has excellent machinability. After machining, the surface can be textured if the end product is to be used in thin film deposition. The graphite is next purified and given an amorphous carbon treatment. This treatment is unique because it does more than coat the surface. It also infiltrates and locks onto the graphite. This treatment provides a hard, abrasion resistant surface that produces no particles. The result is a surface that is grain free, harder than the substrate, but extremely thin.

This nonporous surface does not allow absorption of acids. FABMATE resists attack by hydrofluoric(HF) and most other acids used in the cleaning process.

Information provided by Poco Graphite, Inc.

Available Properties
  • Density
  • Apparent Bulk Density
  • Tensile Strength, Ultimate
  • Flexural Modulus
  • Flexural Strength
  • Compressive Yield Strength
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Inert
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。