MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

AISI 8620 Steel, double quenched and tempered (230°C (450°F)), carburized

 

Subcategory: Low Alloy Steel; AISI 8000 Series Steel; Low Carbon Steel; Metal

Close Analogs: AISI 8620H

Key Words: AFNOR 22 NCD 2, UNI 20 NiCrMo 2, JIS SNCM 21 H, JIS SNCM 21, MIL SPEC MIL-S-16794, SAE J404, SAE J770, DIN 1.6523, AFNOR 20 NCD 2 (France), B.S. 805 H 20 (UK), B.S. 805 M 20 (UK), UNS G86200, AMS 6274, AMS 6276, AMS 6277, ASTM A322, ASTM A331, ASTM A505, ASTM A531

Material Notes:
Double quenched and tempered: carburized at 925°C (1700°F) for 8 hrs., pot cooled, reheated to 845°C (1550°F), quenched in agitated oil, reheated to 800°C (1470°F), quenched in agitated oil, 230°C (450°F) temper. 1.8 mm case depth. Core properties.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell B
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Bulk Modulus
  • Poissons Ratio
  • Machinability
  • Shear Modulus
  • Electrical Resistivity
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。