Aluminum 2011-T6

 

Subcategory: Aluminum Alloy; Nonferrous Metal; 2000 Series Aluminum Alloy

Close Analogs:

Composition Notes:
Aluminum content reported is calculated as remainder.
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 2011-T6; UNS A92011; QQ-A-225/3; NF A-U4Pb (France); DIN AlCuBiPb; BS FC1; AA2011-T6

Material Notes:
Information provided by Alcoa and the references. General 2011 characteristics and uses: Good machinability, especially free-cutting qualities, good mechanical properties. Excellent surface finish capability. The T451 temper offers good deep drilling characteristics.

Uses: Adapters, carburetor parts, clock parts and gears, knobs, camera parts, meter shafts and gears, nozzles, pencil and pen parts, oil line filters, pipe stems and filters, radio parts, screwdriver caps, spindles, telephone parts, TV fittings, tripod fittings, machine parts, hose parts, pipe stems.

Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell A
  • Hardness, Rockwell B
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Fatigue Strength
  • Shear Modulus
  • Shear Strength
  • Electrical Resistivity
  • CTE, linear 68°F
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Annealing Temperature
  • Solution Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。