MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Aluminum 6069-T6, Hot Impact Extruded Cylinder, Minimum Tensile Values

 

Subcategory: Aluminum Alloy; Nonferrous Metal; 6000 Series Aluminum Alloy

Close Analogs:

Composition Notes:
Aluminum content reported is calculated as remainder.
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 6069-T6; UNS A96069

Material Notes:
The alloy 6069 is a new entry to the 6000 series of heat treatable Mg-Si-Cu aluminum alloys. The data available, while not sufficient to establish design mechanical property values, indicate a tensile ultimate and yield strength in the T6 condition about 40% higher than its sister 6061 alloy and essentially equal to the tensile properties of 6013-T6 sheet. Corrosion resistance does not appear to be inferior to 6061. Present applications are high pressure seamless gas containers formed by either hot or cold impact extrusion and tubing for light weight bicycle frames.

Information provided by Northwest Aluminum Company.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Fatigue Strength
  • Fracture Toughness
  • Shear Strength
  • Electrical Resistivity
  • CTE, linear 20°C
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。