Oxygen-free high conductivity Copper, Soft, UNS C10200

 

Subcategory: Copper Alloy; Nonferrous Metal; Wrought Copper

Close Analogs: UNS C10200 - ASTM (flat products) B48, B133, B152, B187, B272, B370, B432, B451, (pipe) B42, B188, (rod) B12, B49, B124,B133, B187, (tubing) B68, B75, B88, B111, B188, B280, B359, B372, B395, B447, (shapes) B124,B133, B187, (wire) B1, B2, B3, B33, B47, B116, B189, B246, B286, B298, B355; C103 (UK); CDA 102 OF; CEN CW009A; Cu/cl NF A53301 (France), ISO Cu-OF R1337; JIS C1020 H3100 - sheet, plate, C1020 H3140 - bar (Japan); QQ-C-576 (flat products), QQ-C-502 (rod, shapes); QQ-C-576 (tube); QQ-C-502, QQ-W-343, MIL-W-3318 (wire)

Key Words: AS 101A 1567 (Australia), OFHC, coining, coppersmithing, ASTM B1, B2, B3, B12, B33, B42, B47, B48, B49, B68, B75, B88, B111, B116, B124, B133, B152, B187, B188, B189, B246, B272, ASTM B286, B298, B355, B359, B370, B372, B395, B432, B451, B447, C103, CDA 102 OF, CEN CW009A, Cu/cl NF A53301, QQ-C-576, CDA 102 OF, C103, ISO Cu-OF R1337, CEN CW008A, OFHC

Material Notes:
UNS C10200 contains a minimum of 99.95 Cu+AgApplications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass to metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers.

Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping.

Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions.

Forms: pipe, plate, rod, shapes, sheet, strip, tube, and wire.

Available Properties
  • Density
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Izod Impact
  • Fatigue Strength
  • Machinability
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 100°C
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。