Domite® Laminated Wear Plate

 

Subcategory: White Cast Iron; Metal; Cast Iron

Key Words: White Cast Iron, ASTM A532 Class II Type B

Material Notes:
Domite® is a white iron metallurgically bonded to a mild steel backing plate, creating a unique material with very high wear resistance and the ductility, toughness, and weldability of mild steel. The cast white iron conforms to ASTM A532 Class II Type B. White Iron is very brittle, exhibiting very little ductility, so tensile and impact tests are not usually a part of the ASTM specification for white iron. This material is normally specified to a hardness criterion. It responds to heat treatment and can be through hardened to a minimum 656 HB or softened to 400 HB for machining and then rehardened. The as cast, heat treated microstructure is uniform throughout with discrete vs. interconnected carbides. It is magnetic.

Applications: wear plates and lip protectors on front-end loaders, transition sections, set bolt protectors, liner plates, crusher hoppers, dump hoppers, vibratory feeders, and conveyor skirt boards.

Information is provided by the manufacturer, Domite Wear Technology Inc.

Available Properties
  • Hardness, Brinell
  • Charpy Impact, Unnotched
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。