Beryllium Copper Nickel 72C Copper Casting Alloy

 

Subcategory: Copper Alloy; Nonferrous Metal

Material Notes:
Alloy 72C is a modified version of beryllium cupro-nickel alloy 71C, its increased beryllium content providing improved castability. Its field of application is the plastic tooling industry. Alloy 72C generally is ceramic mold cast into tooling used for molding flame-retardant plastics containing bromine, bromine-boron, chlorinated paraffins and phosphates, and other halogens. Additionally, alloy 72C tooling is resistant to corrosion by the foaming agents used in structural plastics that generate ammonia at elevated temperatures, as well as to decompositional products of PVC that contain HCI. The good casability of 72C allows it to be cast into tooling of fine detail.

As-cast and aged 3 hours at 510°C.

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 250°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Solution Temperature
  • Aging Temperature
  • Casting Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。