Subscribe to FREE Trade Publications!

Magnesium - AM50A, Thixomolded®

 

Subcategory: Magnesium Alloy; Nonferrous Metal

Close Analogs: Magnesium content calculated as remainder.

Key Words: UNS M10500; ASTM B 94; European EN 1753 MC21220 (Ingot UNS M10501)

Material Notes:
Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heated to high temperatures and injected into a closed die / mold. Parts from the machine usually need no additional machining, finishing or puttying.

Information provided by Parkway Products.

Available Properties
  • Density
  • Hardness, Rockwell E
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Impact Test
  • Electrical Resistivity
  • CTE, linear 68°F
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Across Parting Line Dimensions
  • Flatness Across Largest Dimension
  • Ignition Temperature at One Atmosphere
  • Linear Dimension in same Die Half
  • Mil 117B Salt Spray Corrosion
  • Moving Die Component Tolerances
  • Porosity
  • Shielding Effectiveness 0.020" thk
  • Shielding Effectiveness 0.050" thk
  • Surface Finish
  • Thickness
  • UL94 Flame Exposure Results
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。