Magnesium ZE63A-T6, Cast

 

Subcategory: Magnesium Alloy; Nonferrous Metal

Key Words: UNS M16630; Mg; ASTM B 93 (Ingot UNS M16631)

Material Notes:
Nd content above refers to Nd-rich rare earths. Aerospace and military sand and investment castings used in solution heat treated and artificially aged condition (T6 temper). Has excellent castability and pressure tightness. Especially useful in thin-section castings for applications requiring high mechanical strength and freedom from porosity. Special heat treatment in hydrogen is required to develop mechanical properties, which results in a wall thickness limitation for the castings.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Compressive Yield Strength
  • Compressive Strength
  • Compressive Modulus
  • Poissons Ratio
  • Fracture Toughness
  • Machinability
  • Shear Modulus
  • Electrical Resistivity
  • Heat of Fusion
  • CTE, linear 20°C
  • CTE, linear 100°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Casting Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。