MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Titanium Ti-6Al-4V (Grade 5), Annealed

 

Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy

Close Analogs: 4 other heat treatments of this alloy are listed in MatWeb.

Key Words: Ti-6-4; UNS R56400; ASTM Grade 5 titanium; UNS R56401 (ELI); Ti6Al4V, biomaterials, biomedical implants, biocompatibility

Material Notes:
Information provided by Allvac and the references. Annealing Temperature 700-785ºC. Alpha-Beta Alloy.

Applications: Blades, discs, rings, airframes, fasteners, components. Vessels, cases, hubs, forgings. Biomedical implants.

Biocompatibility: Excellent, especially when direct contact with tissue or bone is required. Ti-6Al-4V's poor shear strength makes it undesirable for bone screws or plates. It also has poor surface wear properties and tends to seize when in sliding contact with itself and other metals. Surface treatments such as nitriding and oxidizing can improve the surface wear properties.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Knoop
  • Hardness, Rockwell C
  • Hardness, Vickers
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Compressive Yield Strength
  • Notched Tensile Strength
  • Ultimate Bearing Strength
  • Bearing Yield Strength
  • Poissons Ratio
  • Charpy Impact
  • Fatigue Strength
  • Fracture Toughness
  • Shear Modulus
  • Shear Strength
  • Electrical Resistivity
  • Magnetic Permeability
  • Magnetic Susceptibility
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Beta Transus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。