Nitinol - NiTi Shape Memory Alloy; Low-Temperature Phase

 

Subcategory: Titanium Alloy; Nickel Alloy; Nonferrous Metal

Close Analogs: MatWeb has a separate entry for the high temperature phase of Nitinol.

Key Words: Titanium Nickel Alloys, SMAs

Material Notes:
Shape Memory Alloys (SMA's) are novel materials which have the ability to return to a predetermined shape when heated. When an SMA is cold, or below its transformation temperature, it has a very low yield strength and can be deformed quite easily into any new shape--which it will retain. However, when the material is heated above its transformation temperature it undergoes a change in crystal structure which causes it to return to its original shape. If the SMA encounters any resistance during this transformation, it can generate extremely large forces. The most common shape memory material is an alloy of nickel and titanium called Nitinol (50 atom% Ni, 50 atom% Ti). This particular alloy has very good electrical and mechanical properties, long fatigue life, and high corrosion resistance.

Information provided by TiNi Alloy Company.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • Magnetic Susceptibility
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。