Tungsten Alloy A95S

 

Subcategory: Tungsten Alloy; Nonferrous Metal; Refractory Metal

Close Analogs: Seven tungsten alloys available from MarkeTech International are listed in MatWeb. See the entry for pure tungsten for a more complete list of property data.

Key Words: MarkeTech International; Ashot Heavy Metals Products

Material Notes:
Ni and Fe in composition above refer to NiFe binder. Data provided by MarkeTech International, representative of Ashot Heavy Metal Products, Co.

MarkeTech represents the Ashot Heavy Metal Products Co., a world leader in sintered tungsten alloy parts. Ashot uses the latest cold isostatic pressing technology and a variety sintering techniques including deformation and heat treatment. Ashot produces a wide variety of tungsten products in a Total Quality Management environment which meets MIL-Q-9858A and ISO 9001. A wide variety of tungsten alloys with tungsten content ranging from 40 to 97% featuring varying degrees of physical and mechanical properties are available in this product line, as are W-Fe, W-Cu and W-Co alloys.

Applications include nuclear and medical radiation shielding for x-ray and radiation therapy shields and industrial applications, aircraft and helicopter rotor balance weights, instrument balance weights, weights for sport equipment, tool damping cutter bars, and high voltage contacts.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。