AK Steel Ferritic Stainless steel 18 SR™

 

Subcategory: Stainless Steel; Metal; Ferritic

Close Analogs: Iron content calculated as remainder

Material Notes:
AK Steel 18 SR™ provides excellent resistance to high temperature scaling - far superior to that of Type 446 stainless steel. This material is readily welded by conventional methods. It is not subject to troublesome embrittlement or loss of corrosion resistance in the heat affected zones that affects many other straight chromium alloys. Typical uses include industrial ovens, blowers, exhaust systems, furnace equipment, heaters, induction furnaces and furnace tubes, annealing boxes, baffle plates, heat exchangers, resistor grids, kiln liners and pyrometer tubes.

Information provided by AK Steel

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Electrical Resistivity
  • Maximum Service Temperature, Air
  • Corrosion Resistance
  • Deep-Drawing Capability rm
  • Strain Hardening Exponent n
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。