AK Steel Ferritic Stainless steel 400

 

Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal; Ferritic

Close Analogs: Iron content calculated as remainder

Material Notes:
AK Steel 400 is one of the most economical chromium ferritic stainless steels. It has corrosion and oxidation resistance comparable to Type 410 stainless steel with good fabricating characteristics. AK Steel 400 contains no titanium, so its surface is free of titanium streaks. This provides improved appearance, and alleviates die wear that may be caused by titanium stabilized chromium steels. AK Steel 400 is non-hardenable by heat treatment because of its low carbon content which also minimizes hardening during welding. Typical applications include heat exchangers, display racks, gas range burner rings, office furniture and other uses where corrosion resistance at minimum cost is important.

Information provided by AK Steel

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。