AK Steel Ferritic Stainless steel 410S

 

Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal; Ferritic

Close Analogs: Iron content calculated as remainder

Material Notes:
AK Steel 410S Stainless Steel is a non-hardening modification of Type 410. A small titanium addition minimizes austenite formation at high temperatures, thereby restricting the alloy`s ability to harden. The result is a soft, ductile condition when the material is rapidly cooled from above the critical temperature. This non-hardening characteristic also retards formation of hardening cracks when the steel is welded. The alloy is completely ferritic in the annealed condition. AK Steel 410S is particularly useful for annealing boxes, quenching racks, oxidation-resistant partitions and other high temperature units. AK Steel 410S is Ferro-magnetic.

Information provided by AK Steel

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Izod Impact
  • Electrical Resistivity
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。