AMPCO METAL AMPCO® M4 Nickel-Aluminum Bronze, Extrusion, ≤ 25.4 mm.

 

Subcategory: Copper Alloy; Nonferrous Metal; Bronze

Close Analogs:

Composition Notes: Copper content calculated from balance.

Key Words: AMS 4590 for extrusions

Material Notes:
The patented process gives AMPCO M4 mechanical properties beyond the range of commercial nickel-aluminum bronzes, comparable to beryllium copper at a lower cost and without the beryllium copper industrial hygiene requirements.

Applications: AMPCO M4 was initially developed as an aircraft specification alloy for gears in retractable landing assemblies, engine spacer bearings and other similar applications. It is rapidly growing in use where higher mechanical properties at elevated temperatures together with corrosion-resistant properties are required. Typical applications include aircraft landing gear bearings and bushings, bending dies (shoes and mandrels) for the tube bending industry, gear wheels and wear/guide plates, etc..

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Compressive Yield Strength
  • Compressive Strength
  • Charpy Impact
  • Fatigue Strength
  • Shear Strength
  • Electrical Resistivity
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。