AMPCO METAL AMPCOLOY® 940 Nickel-Copper, Extrusion, 25 - 50 mm.

 

Subcategory: Copper Alloy; Nickel Alloy; Nonferrous Metal

Close Analogs:

Composition Notes: Copper content calculated from balance.

Key Words: RWMA Class 3

Material Notes:
AMPCOLOY 940 is a patented alloy which meets the demands of users of the RWMA class 3 alloys without Beryllium. In the industrialized countries, stricter health and safety instructions on the use of noxious elements have forced AMPCO to develop this new alloy. It replaces the AMPCOLOY 95 in practically all applications.

Applications: AMPCOLOY 940 is used wherever a good electrical or thermal conductivity is required together with high mechanical properties: Electrode holders and seam welding shafts; Spot welding electrodes, seam welding discs, projection and butt welding dies, principally for stainless steel and Monel; Plunger tips for cold chamber aluminum die casting machines; Parts of moulds for injection moulding of plastics, injection-nozzles and cooling pins; Brake drums for paper winding rolls; Parts for energy engineering

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Compressive Yield Strength
  • Electrical Resistivity
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。