Assab Steels CARMO Cold Work Steel

 

Subcategory: Tool Steel; Chrome-moly Steel; Cold Work Steel; Metal

Material Notes:
CARMO is a high-strength, flame-induction and through hardening steel delivered prehardened to 240-270 HB.
The surface of the steel can be flame-hardened without water cooling to a hardness of 58±2 HRC. The depth of hardness is normally 4-5 mm and the hardened and tempered matrix is a good base for the flame-hardened layer. The steel can be easily repair welded and has a high wear resistance similar to that of A2. The toughness of CARMO is much better than that for the steel types A2 and D2.

CARMO is a cold work tool steel which has been developed together with the automotive industry. Its analysis has been balanced to give one universal tool steel for car body dies instead of the several steel grades (flame hardening and through hardening grades) which are normally used. The steel can be used in the flame-hardened or in the through-hardened condition for blanking and forming of both car body parts (thin sheet) or structural parts (thicker sheet).

Available Properties
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Impact Test
  • CTE, linear 20°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。