Assab Steel 709M Machinery Steel

 

Subcategory: Alloy Steel

Close Analogs: AISI /SAE 4140, DIN 42CrMo4, W.nr. 1.7225, BS 708M42, AFNOR 42CD4, JIS SCM4, SS 2244

Material Notes:
ASSAB 709M is an alloyed machinery steel with high strength in small and medium sizes. As standard ASSAB 705M is supplied tough hardened requiring no further heat treatment. It can be oil hardened to higher mechanical properties.

Applications: ASSAB 709M is suitable for flame and induction hardening. It can also be nitrided or tuffrided to a surface hardness of 600-650 Vickers.

ASSAB 709M is not suitable for welding but can with certain precautions be repair welded.

Typical applications include shafts and other power transmission components as well as high strength bolts.

Available Properties
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Reduction of Area
  • Impact Test
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。