    Bales Nicklon® (Nickel-P.T.F.E.) Mold Coating

     

    Subcategory: Metal Matrix Composite; Nickel Alloy; Ceramic/Metallic Coating

    Material Notes:
    Description: Autocatalytic application provides a uniform layer of 22%-24% PTFE over the deepest ribs and most complex details. It is also corrosion resistant.

    Excellent Release Properties for:

    • Deep Ribs
    • "No Draft" Cores
    • Textured Surfaces
    • Difficult to Eject Polymers

    Information provided by Bales Mold Service Inc.

    Available Properties
    • Hardness, Rockwell C
    • Coefficient of Friction
    • Processing Temperature
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。