Brush Wellman AlBeCast™ IC910 Aluminum Beryllium Composite

 

Subcategory: Metal Matrix Composite; Aluminum Alloy; Nonferrous Metal; Beryllium Alloy

Key Words: Aluminum Beryllium Metal Matrix Composites Alloy

Material Notes:
Aluminum composition above calculated as remainder. Mechanical properties are typical values at RT. AlBeCast™ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stiffness, thermal performance, and weight savings of Al/Be materials. The casting process requires little change from Al or Ti casting.

Please note that there are health hazards associated with beryllium, especially when present as airborne particles generated during processing. As with any material, be aware of hazards and take steps to reduce exposure to a safe level.

Information provided by Brush Wellman.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Compressive Yield Strength
  • Poissons Ratio
  • Fatigue Strength
  • Fracture Toughness
  • Shear Modulus
  • Shear Strength
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。