Brush Wellman Beryllium Nickel Strip - Alloy 390

 

Subcategory: Copper Alloy; Nickel Alloy; Nonferrous Metal; Beryllium Alloy

Key Words: burn in and test socket, bits

Material Notes:
Description: Alloy 390 was specifically designed for high power applications, providing a unique combination of high strength and high conductivity. Increasing power requirements are driving the need for lower conductor resistance to reduce joule heating. Higher thermal conductivity is critical to thermal management. Higher power requirements are creating harsh environments and higher operating temperatures. Alloy 390 provides excellent stress relaxation resistance at elevated temperatures increasing electrical contact reliability. Alloy 390 has good formability making it possible to create small form factor electrical contacts used in computer, telecommunication, automotive and appliance applications. Alloy 390 is available in strip form ranging from 0.003" to 0.010" thick.

Copper content calculated as remainder. Information supplied by Brush Wellman Engineered Materials.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Fatigue Strength
  • Electrical Resistivity
  • Thermal Conductivity
  • Stress Relaxation
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。