UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel

 

Subcategory: Tool Steel; Chrome-moly Steel; Hot Work Steel; Alloy Steel; Metal

Key Words: W.Nr. 1.2344

Material Notes:
Chromium-molybdenum-vanadium alloyed steel

A premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in order to give mechanical properties with maximum isotropy and is certified to meet a minimum Charpy V-notch test result of 10 ft-lbs (13.6 J). Suitable for a wide variety of hot work applications, including tools for high pressure die casting, hot extrusion and press forging, ORVAR® SUPREME also meets or exceeds NADCA 207-97 specifications.

Orvar Supreme is characterized by:

  • High level of resistance to thermal shock and thermal fatigue
  • Good high-temperature strength
  • Excellent toughness and ductility in all directions
  • Good machinability and polishability
  • Excellent through-hardening properties
  • Good dimensional stability during hardening

Information provided by Bohler-Uddeholm

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Charpy Impact
  • CTE, linear, 482°F (250°C)
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。