UDDEHOLM ORVAR® 2M / AISI H13 Hot Work Tool Steel

 

Subcategory: Tool Steel; Chrome-moly Steel; Hot Work Steel; Alloy Steel; Metal

Key Words: W.-Nr. 1.2344

Material Notes:
Chromium-molybdenum-vanadium alloyed steel

ORVAR® 2M / AISI H13 is a conventionally produced hot work tool steel with overall good ductility, toughness, wear resistance, hardenability and machinability. ORVAR 2M from UDDEHOLM is specially processed to provide the best overall product consistency and uniformity available in a conventionally produced AISI H13 tool steel.

ORVAR 2 Microdized is characterized by:

  • Good resistance to abrasion at both low and high temperatures
  • Good toughness and ductility
  • Uniform and high level of machinability and polishability
  • Good high-temperature strength and resistance to thermal fatigue
  • Excellent through-hardening properties

Information provided by Bohler-Uddeholm

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • CTE, linear, 482°F (250°C)
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。