General Grade AISI A2 Cold Work Tool Steel

 

Subcategory: Tool Steel; Cold Work Steel; Alloy Steel; Metal

Key Words: AISI A2; W.-Nr. 1.2363

Material Notes:
Chromium-molybdenum-vanadium alloyed steel

Suitable for medium run tooling. This grade features good machinability, high stability after hardening and good wear resistance. AISI A2 can be supplied in various finishes, including the hot-rolled, pre-machined and fine-machined condition. It is also available in the form of hollow bar and rings.

AISI A2 is characterized by:

  • Good machinability
  • High stability after hardening
  • High compressive strength
  • Good hardenability
  • Good wear resistance

Information provided by Bohler-Uddeholm

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Compressive Yield Strength
  • CTE, linear, 482°F (250°C)
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。