UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel

 

Subcategory: Stainless Steel; Precipitation Hardening Stainless; Alloy Steel; Mold Steel; Metal

Material Notes:

A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-supplied hardness of 34-36 HRC, or a low-temperature aging treatment can increase the hardness up to 50 HRC.

CORRAX® is characterized by:

  • Extremely good dimensional stability during the aging process
  • High uniformity of properties even in large dimensions
  • Very good weldability; no pre-heating necessary
  • No hard "white layer" after EDM
  • Corrosion resistance superior to AISI 420 and AISI 440C

Information provided by Bohler-Uddeholm

Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Compressive Yield Strength
  • Impact Test
  • CTE, linear, 482°F (250°C)
  • Thermal Conductivity at Elevated Temperature
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。