General Grade BeCu Alloy 172 Mold Material

 

Subcategory: Copper Alloy; Beryllium Alloy

Material Notes:
Beryllium copper alloy

A high strength beryllium copper mold alloy with high thermal conductivity. For applications such as pinch offs and neck rings for blow molds, cores and inserts in injection molds and injection nozzles and manifolds for hot runner systems.

BeCu Alloy 172 is characterized by:

  • High thermal conductivity
  • Good corrosion resistance
  • Good polishability
  • Good wear resistance
  • Good resistance to galling
  • Good machinability
  • High strength and hardness
  • Excellent weldability

Information provided by Bohler-Uddeholm

Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Compressive Yield Strength
  • CTE, linear, 482°F (250°C)
  • Specific Heat Capacity
  • Thermal Conductivity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。