Spray Formed Grade WEARTEC SF Cold Work Tool Steel

 

Subcategory: Tool Steel; Chrome-moly Steel; Cold Work Steel; Alloy Steel; Metal

Material Notes:
Chromium-molybdenum-vanadium alloyed steel

The WEARTEC SF steel grade is a very highly alloyed spray formed cold work tool steel with a combination of extremely high wear resistance and a good resistance to cracking. WEARTEC SF is suitable for rolls and rotary knives with very high demands on abrasive wear resistance and carbide applications requiring toughness.

WEARTEC SF is characterized by:

  • Excellent abrasive wear resistance
  • High compressive strength
  • Good toughness
  • Good dimensional stability at heat treatment and in service
  • Very good through hardening properties
  • Very good resistance to tempering back
  • Good WEDM properties
  • Good surface treatment properties

Information provided by Bohler-Uddeholm

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Modulus of Elasticity at Elevated Temperature
  • Compressive Yield Strength
  • CTE, linear, 482°F (250°C)
  • Specific Heat Capacity
  • Thermal Conductivity at Elevated Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。