Carlson Alloy Nitronic 33® Austenitic Stainless Steel

 

Subcategory: Stainless Steel; Alloy Steel; Metal; Austenitic

Key Words: UNS S24000; ASTM XM-29

Material Notes:
General Description

Nitronic 33 is a nitrogen-strengthened austenitic stainless steel that combines high yield strength with excellent toughness and ductility. It’s magnetic permeability remains very low after severe cold working and at cryogenic temperatures.

The alloy is superior to 304 stainless in at least five specific areas: (1) Yield strength in the annealed condition is approximately twice that of 304, (2) it has excellent strength and ductility at cryogenic temperatures, (3)has better stress corrosion cracking resistance than 304, (4) low magnetic permeability is retained at cryogenic temperatures and after severe cold working and, (5) resistance to wear and galling is superior to the standard austenitic stainless steels.

The corrosion resistance of Nitronic 33 is superior to 409 and, in general, is nearly equal to 304. In weak acid solutions, the corrosion resistance of Nitronic 33 approaches that of 304. In more aggressive media Nitronic 33 is somewhat less resistance than 304.

Nitronic 33 is markedly more resistant than 304 and 304L to stress corrosion cracking in hot chloride solutions at lower stress levels. At higher stress levels (approx. 50 ksi and above) they are equal. Like most stainless steels, Nitronic 33 is prone to pitting and crevice corrosion in seawater and other aggressive environments, and should not be used under these conditions unless cathodically protected.

Although Nitronic 33 is considerably stronger than the conventional austenitic stainless steels, the same fabricating equipment and techniques can generally be used.

Applications

  • Cryogenic Service – tanks valves, piping, flanges, and structural supports
  • Abrasion/Wear Resistance – screens, racks, and wear plates
  • Electrical (low magnetic permeability) – conduit shielding, MRI scanner supports, fittings, underground transmission risers and pipe and electronic support members
  • Marine – mine sweeper components and perming piers
  • Nuclear – spent fuel casks (internal supports)
  • Process Equipment – heat exchangers, pressure vessels and piping where 304 is borderline with respect to stress corrosion cracking.

Information provided by Carlson

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell B
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Taber Abrasion, mg/1000 Cycles
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 68°F
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。