Carlson Alloy C 800AT Nickel-Iron-Chromium Alloy

 

Subcategory: Superalloy; Nickel Alloy

Key Words: UNS N08811

Material Notes:
General Description

Carlson Alloy C 800AT is a modification of Carlson Alloy C 800, exhibiting higher creep and rupture strengths. This nickel-iron-chromium alloy has a carbon content restricted to a range of 0.06 to 0.10%. The aluminum plus titanium content of this alloy is also maintained in the upper portion of the standard range (0.85 to 1.20%).

C 800AT is solution-annealed at 2100°F (1500°C). That heat treatment and the compositional restrictions are responsible for this alloy’s improved creep and rupture strengths.

Since the chemistry of C 800AT falls within the range of C 800, there are no significant differences in physical and thermal properties. The major differences between the alloys are in the mechanical properties. (Generally C 800 exhibits higher mechanical properties at room temperature and during short-term exposure to elevated temperatures.) C 800AT displays superior and rupture strengths over long-term exposure to elevated temperatures.

C 800AT offers higher ASME boiler and pressure vessel design stress allowables in creep and rupture test ranges than C 800H.

Applications

  • Chemical and Petrochemical – piping, tubing, pigtails and outlet manifolds in steam/hydrocarbon reforming; tubing for ethylene production; tubing and heaters for oxo-alcohol production; hydrodealkylation units; tubing, flanges and bends for production of vinyl chloride monomer.
  • Thermal Processing – tubing, muffles, retorts and fixtures in heat treating furnaces.
  • Power Generation – tubing in power plant superheaters and reheaters.

Information provided by Carlson

Available Properties
  • Density
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Poissons Ratio
  • Magnetic Permeability
  • Curie Temperature
  • CTE, linear 68°F
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。