CMW® 73 Copper Alloy

 

Subcategory: Copper Alloy; Nonferrous Metal

Material Notes:
CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and wear resistance is obtained in both cast and wrought material largely by means of heat treatment. It is generally useful where high stress is encountered or where high abrasion resistance is desired but where temperatures are not excessive. The annealing temperature is somewhat less than for other heat treatable high strength copper base alloys. The hardness of CMW® 73 material in the fully heat treated condition is sufficiently high to make machining somewhat difficult particularly in drilling and tapping of small holes. Where extensive machining or forming is to be done, CMW® 73 material can be supplied in the solution annealed (soft) condition and then hardened by a simple heat treatment following machining.

CMW® 73 material is useful where extremely high hardness, strength and abrasion resistance is required. It may be advantageously used for certain flash and projection welding dies where high mechanical properties are required but where current density and heat are not excessive. Many of the steel strip flash welders in continuous steel strip mills are equipped with CMW® 73 die facings. The high hardness and abrasion resistance of CMW® 73 material makes it ideally suited for current carrying collets, chucks, bearings and shafts. Current carrying structural members of CMW® 73 material provide extremely high strength.

Information provided by CMW Inc.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Fatigue Strength
  • Electrical Resistivity
  • CTE, linear 100°C
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Softening Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。