Crucible CPM®, High Speed Steel Rex® T15(HS)

 

Subcategory: Tool Steel; High Carbon Steel; Metal

Close Analogs:

Composition:
Iron content calculated as remainder

Key Words: AISI T15 High Speed Steel

Material Notes:
CPM Rex T15 is a super high speed steel made by the Crucible Particle Metallurgy (CPM) process. It is a tungsten type high speed containing high vanadium for excellent abrasion resistance, and cobalt for good red hardness. CPM Rex T15 is ideal for cutting difficult to machine materials where high frictional heating is encountered.

The CPM process results in a homogeneous microstructure with a finer, more uniform carbide distribution imparting superior dimensional stability, grindability and toughness when compared to steels produced by conventional processes. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking.

Information provided by Crucible Specialty Metals.

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell C
  • Modulus of Elasticity
  • Flexural Strength
  • Charpy Impact
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Shrinkage
  • Grindability; Metal Removed/Wheel Worn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。