Special Metals Nickel 205

 

Subcategory: Pure Element; Nickel Alloy; Nonferrous Metal

Key Words: Nickel, Ni, UNS N02205; ASTM F1, F2, F3, F9; SAE AMS 5555; MIL-N-46025; Werkstoff Nr. 2.4061

Material Notes:
Nickel content above includes cobalt. Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic valves, magnetostrictive transducers, lead wires, transistor housings, and battery cases. Standard product forms are sheet, strip and wire.

Data provided by the manufacturer, Special Metals.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Electrical Resistivity
  • Curie Temperature
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。