MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Special Metals MONEL™ Alloy 450

 

Subcategory: Superalloy; Copper Alloy; Nickel Alloy

Key Words: ASME SB-111, SB-171, SB-359, SB-395, SB-466, SB-467, SB-543, Boiler Code Sections III, IV, VIII, IX; SAE J461, J463, MIL-T-15005, MIL-C-15726, MIL-T-16420, MIL-T-22214, Monel Nickel-Copper Alloy, UNS C71500; CDA 715; ASTM B 111, B 122, B 151, B 171, B 359, B 395, B 432, B 466, B 467, B 543, B 552

Material Notes:
Nickel content above includes cobalt; copper content as remainder. A copper-nickel alloy of the 70-30 type having superior weldability. It is resistant to corrosion and bio-fouling in sea water, has good fatigue strength, and has relatively high thermal conductivity. Used for sea-water condensers, condenser plates, distiller tubes, evaporator and heat exchanger tubes, and salt-water piping. Standard product forms are round, hexagon, flats, forging stock, pipe, tube, plate, sheet, and wire.

Data provided by the manufacturer, Special Metals.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Electrical Resistivity
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。