Special Metals INCONEL® Alloy 625

 

Subcategory: Superalloy; Nickel Base

Key Words: ASME SB-443, SB-444, SB-446, SB-564, Boiler Code Sections I, III, VIII, IX; AFNOR NC 22 D Nb; VdTUV 499, AMS 5581, AMS 5599, AMS 5666, AMS 5837; DIN 17744, 17750-17752, 17754; Werkstoff Nr. 2.4856; NACE MR-01-75, UNS N06625; BS 3072, 3074, 3076 (NA21); ASTM B443, ASTM B444, ASTM B446, ASTM B564, ASTM B704, ASTM B705, ASTM B751

Material Notes:
Niobium content above includes tantalum. A nickel-chromium-molybdenum alloy with an addition of niobium that acts with the molybdenum to stiffen the alloy's matrix and thereby provide high strength without a strengthening heat treatment. The alloy resists a wide range of severely corrosive environments and is especially resistant to pitting and crevice corrosion. Used in chemical processing, aerospace and marine engineering, pollution-control equipment, and nuclear reactors. Standard product forms are round, flats, forging stock, extruded section, pipe, tube, plate, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Electrical Resistivity
  • Magnetic Permeability
  • Curie Temperature
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。