Special Metals INCOLOY® Alloy 330

 

Subcategory: Superalloy; Iron Base

Key Words: SAE AMS 5592, 5716; SAE J405, J412, UNS N08330; ASTM B 511, B 512, B 535, B 536, B 546, B 710; ASME SB-511, SB-536, SB-710, Boiler Code Sections I, VIII, IX

Material Notes:
Iron content as remainder. A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospheres. The alloy's austenitic microstructure remains stable during long-time exposure to high temperature. Used in industrial heating for furnace muffles, retorts, and conveyor systems and for heat-treating baskets and fixtures. Standard product forms are round, flats, forging stock, plate, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。