Special Metals NILO™ Alloy 42 Controlled-Expansion Alloy

 

Subcategory: Superalloy; Iron Base

Key Words: UNS K94100; ASTM F 30, B 753; DIN 17745; S.E.W. 385; Werkstoff Nr. 1.3917; AFNOR NF A54-301

Material Notes:
Iron content as remainder; nickel content is nominal value and is adjusted to meet expansion requirements. Inflection point 370°C. A nickel-iron controlled-expansion alloy containing 42% nickel. It has a low and nominally constant coefficient of thermal expansion from room temperature to about 570°F (300°C). Used for semiconductor lead frames in integrated circuits, bi-metal thermostat strip, thermostat rods, for ceramic-to-metal seals with alumina ceramics, and various glass-to-metal seals such as the core of copper-clad wire for sealing into glass envelopes of electric bulbs, radio valves, television tubes, and fluorescent lights. Standard product forms are tube, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • Thermal Conductivity
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。